Aluminum 6005 T1 Mechanical Properties
Designation 6005, wrought Condition T1 (Cooled from elevated temperature shaping process and naturally aged) UNS number A96005 EN name EN AW-6005 Aluminum 6005 T1 Mechanical properties Young’s modulus 67.5 – 71 GPa Specific stiffness 24.9 – 26.3 MN.m/kg Yield strength (elastic limit) 105 – 122 MPa Tensile strength 170 – 198 … Continue reading Aluminum 6005 T1 Mechanical Properties