Aluminum 6005 T5 Mechanical Properties
Designation 6005, wrought Condition T5 (Cooled from an elevated-temperature shaping process and artificially aged) UNS number A96005 EN name EN AW-6005 Aluminum 6005 T5 Mechanical Properties Young’s modulus 67.4 – 70.9 GPa Specific stiffness 24.9 – 26.3 MN.m/kg Yield strength (elastic limit) 240 – 280 MPa Tensile strength 260 – 303 … Continue reading Aluminum 6005 T5 Mechanical Properties