Aluminum 355.0 permanent mold cast T6 Mechanical Properties
| Property | Range |
|---|---|
| Young’s Modulus | 68.6 – 71.4 GPa |
| Specific Stiffness | 25.3 – 26.4 MN.m/kg |
| Yield Strength (Elastic Limit) | 165 – 182 MPa |
| Tensile Strength | 259 – 286 MPa |
| Specific Strength | 60.9 – 67.3 kN.m/kg |
| Elongation | 2.2 – 2.6 % strain |
| Compressive Strength | 109 – 121 MPa |
| Flexural Modulus | 68.6 – 71.4 GPa |
| Flexural Strength (Modulus of Rupture) | 165 – 182 MPa |
| Shear Modulus | 25.6 – 27 GPa |
| Bulk Modulus | 64.2 – 73.5 GPa |
| Poisson’s Ratio | 0.322 – 0.338 |
| Shape Factor | 33 |
| Hardness (Vickers) | 100 – 110 HV |
| Elastic Stored Energy (Springs) | 195 – 237 kJ/m³ |
| Fatigue Strength at 10^7 cycles | 63 – 77 MPa |
| Fatigue Strength Model (Stress Range) | 60.8 – 79.9 MPa |
| EN AC-Al Si5Cu1Mg Mechanical Properties |