Aluminum, 355.0, permanent mold cast, T6 | General Information

Aluminum 355.0 permanent mold cast T6 General Information

PropertyDetails
Designation355.0 (Aluminum Association)
ConditionT6 (Solution heat-treated and artificially aged)
UNS NumberA03550
EN NumberEN AC-45300 / EN AC-Al Si5Cu1Mg

Typical Uses

Typical Uses of Aluminum 355.0 permanent mold cast T6
High strength alloy: engine cooling fans, clutch housings, high-speed rotating parts, structural aerospace components, compressor cases, machine parts