Aluminum 355.0 permanent mold cast T6 Standards with Similar Compositions
| Region | Standards |
|---|---|
| Canada | SC51N to CSA HA.10, SG51N to CSA HA.9 |
| Europe | EN AB-45300 to CEN EN 1676, EN AC-45300 to CEN EN 1706 |
| International | AlSi5Cu1Mg to ISO 3522 |
| Japan | AC4D to JIS H5202, AC4D.1 to JIS H2211 |
| Spain | L-2571 to UNE 38-203, L-2571 to UNE 38-266 |
| UK | LM16 to BS 1490 |
| USA | 355, 355 to ASTM B108, 355 to ASTM B26/B26M, 355 to ASTM B618, 355.1, 355.1 to ASTM B179, A03550 to SAE J452, UNS A03550, UNS A03551 |
| Tradenames | USCO 5-W |
| Aluminum 355.0 permanent mold cast T6 Standards with Similar Compositions |