Aluminum, 355.0, permanent mold cast, T6 | Composition

Aluminum 355.0 permanent mold cast T6 Composition Overview

PropertyDetails
Compositional SummaryAl90-94 / Si4.5-5.5 / Cu1-1.5 / Mg0.4-0.6 (impurities: Fe<0.6, Mn<0.5, Zn<0.35, Cr<0.25, Ti<0.25, Other<0.15)
Material FamilyMetal (non-ferrous)
Base MaterialAl (Aluminum)

Aluminum 355.0 permanent mold cast T6 Composition Detail

ElementPercentage (%)
Al (Aluminum)90.3 – 94.1
Cr (Chromium)0 – 0.25
Cu (Copper)1 – 1.5
Fe (Iron)0 – 0.6
Mg (Magnesium)0.4 – 0.6
Mn (Manganese)0 – 0.5
Si (Silicon)4.5 – 5.5
Ti (Titanium)0 – 0.25
Zn (Zinc)0 – 0.35
Other0 – 0.15
EN AC-Al Si5Cu1Mg Composition Detail