Aluminum 354.0 cast T6 Standards with Similar Compositions
| Country | Standard |
| USA | 354 |
| 354 to ASTM B108 | |
| 354 to ASTM B686 | |
| 354 to MIL A-21180C | |
| 354.1 | |
| 354.1 to ASTM B179 | |
| 354.1 to QQ A-371F | |
| 354.2 | |
| A03540 to SAE J452 | |
| UNS A03540 | |
| UNS A03541 | |
| Aluminum 354.0 cast T6 Equivalent Grades |
| Aluminum 354.0 cast T6 Tradenames |
|---|
| TA-354, TECHNI-CAST A-354 |
| Tradenames of Aluminum 354.0 cast T6 |