| Property | Value Range | Units |
|---|---|---|
| Young’s modulus | 73 – 76.7 | GPa |
| Specific stiffness | 26.1 – 27.5 | MN·m/kg |
| Yield strength (elastic limit) | 244 – 270 | MPa |
| Tensile strength | 304 – 336 | MPa |
| Specific strength | 87.3 – 96.6 | kN·m/kg |
| Elongation | 2 – 3 | % strain |
| Compressive strength | 244 – 270 | MPa |
| Flexural modulus | 73 – 76.7 | GPa |
| Flexural strength (modulus of rupture) | 244 – 270 | MPa |
| Shear modulus | 28 – 29.4 | GPa |
| Bulk modulus | 71.7 – 75.4 | GPa |
| Poisson’s ratio | 0.33 – 0.343 | |
| Shape factor | 27 | |
| Hardness – Vickers | 110 – 120 | HV |
| Elastic stored energy (springs) | 398 – 487 | kJ/m³ |
| Fatigue strength at 10⁷ cycles | 132 – 154 | MPa |
| Fatigue strength model (stress range) | 126 – 161 | MPa |