Aluminum, 354.0, cast, T6 | Mechanical Properties
Aluminum 354.0 cast T6 Mechanical Properties Property Value Range Units Young’s modulus 73 – 76.7 GPa Specific stiffness 26.1 – 27.5 MN·m/kg Yield strength (elastic limit) 244 – 270 MPa Tensile strength 304 – 336 MPa Specific strength 87.3 – 96.6 kN·m/kg Elongation 2 – 3 % strain Compressive strength 244 – 270 MPa Flexural … Continue reading Aluminum, 354.0, cast, T6 | Mechanical Properties