Aluminum, 354.0, cast, T6 | Composition
Compositional Summary for Aluminum 354.0 T6 Composition Summary Details Al87-89 / Si8.6-9.4 / Cu1.6-2 / Mg0.4-0.6 Impurities: Fe<0.2, Ti<0.2, Mn<0.1, Zn<0.1 Aluminum, 354.0, cast, T6 Composition Summary Material Family Base Material Metal (non-ferrous) Al (Aluminum) Composition Detail of Aluminum 354.0 T6 Element Composition Range (%) Al (Aluminum) 87.4 – 89.4 Cu (Copper) 1.6 – 2.0 … Continue reading Aluminum, 354.0, cast, T6 | Composition