General Information
| Property | Value |
|---|---|
| Designation | 332.0 (Aluminum Association) |
| Condition | T5 (Cooled from an elevated-temperature shaping process and artificially aged) |
| UNS Number | A03320 |
| Typical Uses | High-temperature alloy: pistons, cylinder heads, gear housings, other engine parts |
| Aluminum, 332.0, permanent mold cast, T5 | General Information | UNS A03320 | General Information |
Aluminum, 332.0, permanent mold cast, T5 | General Information
Aluminum, 332.0, permanent mold cast, T5 | Composition
Aluminum, 332.0, permanent mold cast, T5 | Mechanical Properties
Aluminum, 332.0, permanent mold cast, T5 | Equivalent Grades