Aluminum, 332.0, permanent mold cast, T5 | Equivalent Grades

Standards with Similar Compositions

RegionStandard
AustraliaAA305 to AS 1874
India4525 to IS 202 or 617
JapanAC8C to JIS H5202, AC8C.1 to JIS H2211, C8CS to JIS H2117
UKLM26 to BS 1490
USA332, 332 to ASTM B108, 332.1, 332.1 to ASTM B179, A03320 to SAE J452, F132.0 to QQ A-596, F332.1 to QQ A-371F, F332.2 to QQ A-371F, UNS A03320, UNS A03321
Aluminum, 332.0, permanent mold cast, T5 | Standards with Similar Compositions
UNS A03320 Standards with Similar Compositions

Tradenames

Tradenames
AFFIMET AL-SI 10 CU 3 MG
AS 305
GM-4334M
LM 26
Aluminum, 332.0, permanent mold cast, T5 | Tradenames
UNS A03320 Tradenames

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey