Composition Overview
| Compositional Summary |
|---|
| Al: 80-89%, Si: 8.5-10%, Cu: 2-4%, Mg: 0.5-1.5% (Impurities: Fe < 1.2%, Zn < 1%, Mn < 0.5%, Ni < 0.5%, Ti < 0.25%, Other < 0.5%) |
| Aluminum, 332.0, permanent mold cast, T5 | Compositional Summary UNS A03320 Compositional Summary |
Material Family
| Category | Details |
|---|---|
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
Composition Detail
| Element | Min (%) | Max (%) |
|---|---|---|
| Al (Aluminum) | 80 | 89 |
| Si (Silicon) | 8.5 | 10 |
| Cu (Copper) | 2 | 4 |
| Mg (Magnesium) | 0.5 | 1.5 |
| Fe (Iron) | 0 | 1.2 |
| Zn (Zinc) | 0 | 1 |
| Mn (Manganese) | 0 | 0.5 |
| Ni (Nickel) | 0 | 0.5 |
| Ti (Titanium) | 0 | 0.25 |
| Other | 0 | 0.5 |
| Aluminum, 332.0, permanent mold cast, T5 | Composition Detail | UNS A03320 Composition Detail |
Aluminum, 332.0, permanent mold cast, T5 | General Information
Aluminum, 332.0, permanent mold cast, T5 | Composition
Aluminum, 332.0, permanent mold cast, T5 | Mechanical Properties
Aluminum, 332.0, permanent mold cast, T5 | Equivalent Grades