General Information
| Category | Details |
|---|---|
| Designation | 319.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A03190 |
| EN Number | EN AC-45200 / EN AC-Al Si6Cu4 |
| Tradenames | Allcast |
| Aluminum, 319.0, sand cast, T6 | General iInformation | EN AC-45200 / EN AC-Al Si6Cu4 T6 | General information |
Typical Uses
| Application |
|---|
| Engine crankcases |
| Gasoline and oil tanks |
| Oil pans |
| Typewriter frames |
| Engine parts |
| Aluminum, 319.0, sand cast, T6 | Typical Uses EN AC-45200 / EN AC-Al Si6Cu4 T6 | Typical Uses UNS A03190 Typical Uses |
Aluminum, 319.0, sand cast, T6 | General Information
Aluminum, 319.0, sand cast, T6 | Composition
Aluminum, 319.0, sand cast, T6 | Mechanical Properties
Aluminum, 319.0, sand cast, T6 | Equivalent Grades
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey