PropertyMinimumMaximumUnit
Young’s Modulus72.575.5GPa
Specific Stiffness25.927.1MN.m/kg
Yield Strength (Elastic Limit)118130MPa
Tensile Strength186205MPa
Specific Strength42.146.6kN.m/kg
Elongation22.4% strain
Compressive Strength118130MPa
Flexural Modulus72.575.5GPa
Flexural Strength (Modulus of Rupture)124136MPa
Shear Modulus27.128.6GPa
Bulk Modulus67.977.7GPa
Poisson’s Ratio0.3220.338–
Shape Factor39––
Hardness (Vickers)8391HV
Elastic Stored Energy (Springs)93.8115kJ/m³
Fatigue Strength at 10⁷ Cycles6377MPa
Fatigue Strength Model (Stress Range)60.979.7MPa
Aluminum, 319.0, sand cast, F | Mechanical PropertiesEN AC-45200 / EN AC-Al Si6Cu4 | Mechanical Properties

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey