Aluminum, 319.0, sand cast, F | Composition

Composition Overview

CategoryDetails
Compositional SummaryAl 86-92 / Si 5.5-6.5 / Cu 3-4 (impurities: Fe < 1, Zn < 1, Mn < 0.5, Ni < 0.35, Ti < 0.25, Mg < 0.1, Other < 0.5)
Material FamilyMetal (non-ferrous)
Base MaterialAl (Aluminum)
Aluminum, 319.0, sand cast, F | Composition OverviewEN AC-45200 / EN AC-Al Si6Cu4 | Composition Overview

Composition Details

ElementMinimum (%)Maximum (%)
Al (Aluminum)85.891.5
Cu (Copper)34
Fe (Iron)01
Mg (Magnesium)00.1
Mn (Manganese)00.5
Ni (Nickel)00.35
Si (Silicon)5.56.5
Ti (Titanium)00.25
Zn (Zinc)01
Other00.5
Aluminum, 319.0, sand cast, F | Composition DetailsEN AC-45200 / EN AC-Al Si6Cu4 | Composition Details