Aluminum, 319.0, sand cast, F | Equivalent Grades

CountryStandard/Specification
AustraliaAA339 to AS 1874
India4320 to IS 202 or 617
Italy7369/4SG-AlSi6Cu4 to UNI
JapanAC2B to JIS H5202, AC2B.1 to JIS H2211
USA319, 319 to ASTM B108, 319 to ASTM B26/B26M, 319 to ASTM B618, 319.1, 319.1 to ASTM B179, 319.1 to QQ A-371F,

319.2 to QQ A-371F, A03190 to SAE J452, A319.0, A319.1, UNS A03190, UNS A03191, UNS A13190, UNS A13191
RussiaGOST 2685 AL6
Aluminum, 319.0, sand cast, F | Equivalent Grades EN AC-45200 / EN AC-Al Si6Cu4 | Equivalent Grades

Tradenames
ALLCAST 51
GM-4227 M
USCO 319.1

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey