Aluminum, 319.0, permanent mold cast, T6 | Mechanical Properties

Mechanical Properties

PropertyMinimumMaximumUnit
Young’s Modulus72.575.5GPa
Specific Stiffness25.927.1MN.m/kg
Yield Strength (Elastic Limit)157173MPa
Tensile Strength242251MPa
Specific Strength5662kN.m/kg
Elongation22.4% strain
Compressive Strength157173MPa
Flexural Modulus72.575.5GPa
Flexural Strength (Modulus of Rupture)165182MPa
Shear Modulus27.128.6GPa
Bulk Modulus67.977.7GPa
Poisson’s Ratio0.3220.338–
Shape Factor35––
Hardness (Vickers)105116HV
Elastic Stored Energy (Springs)166203kJ/m³
Fatigue Strength at 10⁷ Cycles74.791.3MPa
Fatigue Strength Model (Stress Range)74.391.8MPa
Aluminum, 319.0, permanent mold cast, T6 | Mechanical PropertiesEN AC-45200 / EN AC-Al Si6Cu4 Mechanical Properties

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey