Composition Overview
| Category | Details |
|---|---|
| Compositional Summary | Al 86-92 / Si 5.5-6.5 / Cu 3-4 (impurities: Fe < 1, Zn < 1, Mn < 0.5, Ni < 0.35, Ti < 0.25, Mg < 0.1, Other < 0.5) |
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
| Aluminum, 319.0, permanent mold cast, T6 | Composition Overview | EN AC-45200 / EN AC-Al Si6Cu4 Composition Overview |
Composition Details
| Element | Minimum (%) | Maximum (%) |
|---|---|---|
| Al (Aluminum) | 85.8 | 91.5 |
| Cu (Copper) | 3 | 4 |
| Fe (Iron) | 0 | 1 |
| Mg (Magnesium) | 0 | 0.1 |
| Mn (Manganese) | 0 | 0.5 |
| Ni (Nickel) | 0 | 0.35 |
| Si (Silicon) | 5.5 | 6.5 |
| Ti (Titanium) | 0 | 0.25 |
| Zn (Zinc) | 0 | 1 |
| Other | 0 | 0.5 |
| Aluminum, 319.0, permanent mold cast, T6 | Composition Details | EN AC-45200 / EN AC-Al Si6Cu4 Composition Details |
Aluminum, 319.0, permanent mold cast, T6 | General Information
Aluminum, 319.0, permanent mold cast, T6 | Composition
Aluminum, 319.0, permanent mold cast, T6 | Mechanical Properties
Aluminum, 319.0, permanent mold cast, T6 | Equivalent Grades
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey