General Information
| Category | Details |
|---|---|
| Designation | 319.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A03190 |
| EN Number | EN AC-45200 / EN AC-Al Si6Cu4 |
Tradenames
| Tradename |
|---|
| Allcast |
Typical Uses
| Applications |
|---|
| Engine crankcases |
| Gasoline and oil tanks |
| Oil pans |
| Typewriter frames |
| Engine parts |
Aluminum, 319.0, permanent mold cast, T6 | General Information
Aluminum, 319.0, permanent mold cast, T6 | Composition
Aluminum, 319.0, permanent mold cast, T6 | Mechanical Properties
Aluminum, 319.0, permanent mold cast, T6 | Equivalent Grades