| AISI 1030, Carbon steel | Equivalent Grades |
|---|---|
| UNS number | G10300 |
| US name | ASTM 1030, ASTM 1029, ASTM G10290, ASME G10300, ~ASTM M1031, ~ASTM FPB, ~ASTM C2, ~ASTM A-1, ~ASTM 36, ~ASTM 1029, ~ASME G10290 |
| UK name | 080M30 to BS 970/1 |
| Germany name | DIN 1654(89) 28B2 |
| JIS (Japanese) name | ~STPG 410, ~STKM15C, ~STKM15A, ~STKM14C, ~STKM14B, ~STKM14A, ~SPHT 4 |
Tradenames of AISI 1030, Carbon steel : CS1030, D-M-E NO. 1, GREDE 34, JESSOP STEEL A-4 (S M-30), NITRIX 1473, V3, V3/1
| Standards with similar compositions: |
|---|
| IAS IRAM 1030 (Argentina) |
| ONORM M3110 RC30 (Austria) |
| ONORM M3167 C355P (Austria) |
| EN 10083/1(91)A1(96) 1.1178 (Europe) |
| EN 10083/1(91)A1(96) 1.1179 (Europe) |
| EN 10083/1(91)A1(96) C30E (Europe) |
| EN 10083/1(91)A1(96) C30R (Europe) |
| EN 10083/2(91)A1(96) 1.0528 (Europe) |
| EN 10083/2(91)A1(96) C30 (Europe) |
| BDS 5785(83) 30 (Bulgaria) |
| BDS 5785(83) 30G (Bulgaria) |
| GB 13237(91) 30 (China) |
| GB 3275(91) 30 (China) |
| GB 3522(83) 30 (China) |
| GB 5953(86) ML 30 (China) |
| GB 6478(86) ML 30 (China) |
| GB 699(88) 30 (China) |
| GB 710(91) 30 (China) |
| GB/T 3078(94) 30 (China) |
| CSN 412031 12031 (Czech Republic) |
| SFS 1205(74) SFS1205 (Finland) |
| SFS 1212(80) SFS1210 (Finland) |
| SFS 1212(80) SFS1212 (Finland) |
| SFS 1214(83) SFS1214 (Finland) |
| SFS 2148 Fe55 (Finland) |
| AFNOR NFA35552 XC32 (France) |
| AFNOR NFA35553 XC32 (France) |
| AFNOR NFA36102(93) 25B3 (France) |
| AFNOR NFA36102(93) 25B3RR (France) |
| DIN 1654(89) 28B2 (Germany) |
| DIN 1654(89) WNr 1.5510 (Germany) |
| DIN 17140 D30-2 (Germany) |
| DIN EN 10083(91) C30E (Germany) |
| DIN EN 10083(91) Ck30 (Germany) |
| DIN EN 10083(91) Cm30 (Germany) |
| DIN EN 10083(91) WNr 1.0528 (Germany) |
| DIN EN 10083(91) WNr 1.1178 (Germany) |
| DIN EN 10083(91) WNr 1.1179 (Germany) |
| MSZ 3156(84) D (Hungary) |
| MSZ 3156(84) E (Hungary) |
| MSZ 61(78) C30 (Hungary) |
| MSZ 61(85) C30 (Hungary) |
| MSZ 61(85) C30E (Hungary) |
| IS 1570/2(79) 30C8 (India) |
| IS 1570/2(79) C30 (India) |
| IS 5517 C30 (India) |
| UNI 5332 C30 (Italy) |
| UNI 5598(71) 1CD30 (Italy) |
| UNI 5598(71) 3CD30 (Italy) |
| UNI 6403(86) C30 (Italy) |
| UNI 6783 Fe50-3 (Italy) |
| UNI 7065(72) C30 (Italy) |
| UNI 7065(72) C31 (Italy) |
| UNI 7845(78) C30 (Italy) |
| UNI 7874(79) C30 (Italy) |
| JIS G3311(88) S30CM (Japan) |
| JIS G3445(88) STKM15A (Japan) |
| JIS G3445(88) STKM15C (Japan) |
| JIS G3507(91) SWRCH30K (Japan) |
| JIS G4051(79) S30C (Japan) |
| JIS G4051(79) S33C (Japan) |
| DGN B-203 1030 (Mexico) |
| NMX-B-178(90) Grade B (Mexico) |
| NMX-B-197(85) Grade 1 (Mexico) |
| NMX-B-197(85) Grade 6 (Mexico) |
| NMX-B-201(68) 1030 (Mexico) |
| NMX-B-301(86) 1030 (Mexico) |
| NS SE3 (Norway) |
| AS 1442 CS1030 (NSW Australia) |
| AS 1442 K1030 (NSW Australia) |
| AS 1442 S1030 (NSW Australia) |
| AS 1442(92) 1030 (NSW Australia) |
| AS 1442(92) M1030 (NSW Australia) |
| AS 1443 CS1030 (NSW Australia) |
| AS 1443 K1030 (NSW Australia) |
| AS 1443 S1030 (NSW Australia) |
| AS 1443(94) 1030 (NSW Australia) |
| AS 1443(94) D4 (NSW Australia) |
| AS 1443(94) M1030 (NSW Australia) |
| AS 1443(94) T4 (NSW Australia) |
| PNH84019 30 (Poland) |
| PNH84023/06 34GS (Poland) |
| PNH84023/07 R34GS (Poland) |
| STAS 880(88) OLC30 (Romania) |
| STAS 880(88) OLC30S (Romania) |
| STAS 880(88) OLC30X (Romania) |
| STAS 880(88) OLC30XS (Romania) |
| GOST 2Kh (Russian Federation) |
| GOST 5K (Russian Federation) |
| GOST 5sp (Russian Federation) |
| GOST KSt5 (Russian Federation) |
| GOST KSt5kp (Russian Federation) |
| GOST KSt5ps (Russian Federation) |
| GOST M31 (Russian Federation) |
| GOST M31A (Russian Federation) |
| GOST MSt5 (Russian Federation) |
| GOST St5 (Russian Federation) |
| GOST St5K (Russian Federation) |
| GOST VK (Russian Federation) |
| GOST 1050 30 (Russian Federation) |
| GOST 1050(88) 30 (Russian Federation) |
| GOST 380 BSt5sp (Russian Federation) |
| GOST 380 St5S (Russian Federation) |
| GOST 4543 30G (Russian Federation) |
| GOST 977 30L-II (Russian Federation) |
| GOST 977 30L-III (Russian Federation) |
| SS 141505 1505 (Sweden) |
| ISO 683-1(87) C30 (International) |
| ISO 683-1(87) C30E4 (International) |
| ISO 683-1(87) C30M2 (International) |
| ISO 683-18(96) C30 (International) |
| ISO 683-18(96) C30E4 (International) |
| ISO 683-18(96) C30M2 (International) |
| ISO R683-1 C30e (International) |
| ISO R683-3(70) C30ea (International) |
| ISO R683-3(70) C30eb (International) |
| TS 302 Fe55.2 (Turkey) |
| TS 346 Fe55 (Turkey) |
| TS 909(86) UDK629.14.423/Fe42 (Turkey) |
| TS 911(86) UDK669.14.423/Fe50 (Turkey) |
| TS 912(86) UDK669.14.423/Fe42 (Turkey) |
| TS 913(86) UDK669.14.423/Fe42 (Turkey) |
| BS 1449/1(91) 30CS (United Kingdom) |
| BS 1449/1(91) 30HS (United Kingdom) |
| BS 970/1(83) 060A30 (United Kingdom) |
| BS 970/1(83) 080A30 (United Kingdom) |
| BS 970/1(83) 080M30 (United Kingdom) |
| BS 970/3(91) 080M30 (United Kingdom) |
| ASTM A108(95) 1030 (USA) |
| ASTM A29/A29M(93) 1030 (USA) |
| ASTM A510(96) 1030 (USA) |
| ASTM A512(96) 1030 (USA) |
| ASTM A513(97a) 1030 (USA) |
| ASTM A519(96) 1030 (USA) |
| ASTM A575(96) M1031 (USA) |
| ASTM A576(95) 1030 (USA) |
| ASTM A682/A682M(98) 1030 (USA) |
| ASTM A684A684M(86) 1030 (USA) |
| ASTM A830/A830M(98) 1030 (USA) |
| ASTM A866(94) 1030 (USA) |
| FED QQ-S-635B(88) C1030 (USA) |
| FED QQ-S-700D(91) C1030 (USA) |
| MIL-F-20670B(61) (USA) |
| MIL-S-10520D(AR)(88) 2 (USA) |
| MIL-S-11310E(76) CS1030 (USA) |
| MIL-S-16788A(86) C3 (USA) |
| MIL-S-3289B(84) (USA) |
| MIL-S-46070 1030 (USA) |
| SAE J1397(92) 1030 (USA) |
| SAE J403(95) 1030 (USA) |
| AISI 1030 (USA) |
| COPANT 330 1030 (Venezuela) |
| COPANT 331 1030 (Venezuela) |
| COPANT 333 1030 (Venezuela) |
| COPANT 514 1030 (Venezuela) |
| C.0545 (Yugoslavia) |
- China:
ML30Mn to GB/T 6478 - India:
30C8 to IS 1570/2/1, 35C8 to IS 1570/2/1, C30 to IS 1570/2/1, C30 to IS 6967, C35Mn75 to IS 1570/2/1, CDS-4 to IS3074 - Mexico:
1029 to NMX-B-301, 1030 to NMX-B-201, 1030 to NMX-B-203-SCFI, 1030 to NMX-B-301, 1034 to NMX-B-301, 1035 to NMX-B-203-SCFI, 1035 to NMX-B-301, 1037 to NMX-B-301 - Pan America:
1029 to COPANT 333, 1030 to COPANT 330, 1030 to COPANT 331, 1030 to COPANT 333, 1034 to COPANT 333, 1035 to COPANT 330, 1035 to COPANT 331, 1035 to COPANT 333 - Sweden:
1550 to SS 141550 - UK:
080M30 to BS 970/1 - USA:
1029, 1029 to ASTM A29/A29M, 1029 to SAE J403, 1030, 1030 to ASTM A29/A29M, 1030 to ASTM A512-96, 1030 to ASTM A513, 1030 to ASTM A519, 1030 to ASTM A568/A568M, 1030 to SAE J403, 1033, 1033 to ASTM A513, 1033 to ASTM A568/A568M, 1033 to SAE J403, 1034, 1034 to ASTM A29/A29M, 1035, 1035 Class A to ASTM A311/A311M, 1035 to ASTM A29/A29M, 1035 to ASTM A512-96, 1035 to ASTM A513, 1035 to ASTM A519, 1035 to ASTM A568/A568M, 1035 to DoD-F-24669/1, 1035 to FED QQ-W-461H, 1035 to SAE J403, 1037, 1037 to ASTM, A29/A29M, 1037 to ASTM A568/A568M, 1037 to SAE J1249, 1037 to SAE J403, C1030 to FED QQ-S-635B, C1030
to FED QQ-S-700D, C1035 to FED QQ-S-635B, C1035 to FED QQ-S-700D, C3 to MIL-S-16788A, CS1030 to MIL-S-11310E, E to MIL-T-20157, G10290 to ASTM A510/A510M, G10290 to ASTM A576-90b, G10300 to ASTM A510/A510M, G10300 to ASTM A576-90b, G10300 to ASTM A830/A830M, G10330 to ASTM A830/A830M, G10340 to ASTM A510/A510M, G10350 to ASTM A510/A510M, G10350 to ASTM A576-90b, G10350 to ASTM A830/A830M, G10370 to ASTM A510/A510M, G10370 to ASTM A576-90b, G10370 to ASTM A830/A830M, MIL-S-3289B to MIL-S-3289B, UNS G10290, UNS G10300, UNS G10300 to UNS, UNS G10330, UNS G10340, UNS G10350, UNS G10350 to UNS, UNS G10370, UNS G10370 to UNS, UNS K02901