AISI 1030 Annealed Carbon steel | Mechanical Properties
AISI 1030 Annealed Carbon Steel Mechanical Properties Values Young’s modulus 208 – 216 GPa Specific stiffness 26.5 – 27.5 MN.m/kg Yield strength (elastic limit) 305 – 375 MPa Tensile strength 410 – 515 MPa Specific strength 38.8 – 47.8 kN.m/kg Elongation 25 – 38 % strain Compressive strength * 305 – 375 MPa Flexural modulus … Continue reading AISI 1030 Annealed Carbon steel | Mechanical Properties