Aluminum 356.0 sand cast T6 General Information
| Property | Value |
|---|---|
| Designation | 356.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A03560 |
| EN Number | EN AC-42000 / EN AC-Al Si7Mg |
| Aluminum 356.0 sand cast T6 General Information |
Typical uses of Aluminum 356.0, sand cast, T6:
| Typical Uses |
|---|
| High strength alloy for the automotive industry: |
| Space frames |
| Wheels |
| Axle and differential housings |
| Pumps |
| Meters |
| Differential housings |
| Intake manifolds |
| Electronic cases |
| Fuel pumps |
| Typical uses of Aluminum 356.0, sand cast, T6 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey