Aluminum, 356.0, sand cast, T6 | Mechanical Properties
Mechanical properties of Aluminum 356.0, sand cast, T6 Property Value Range Young’s modulus 71.5 – 74.5 GPa Specific stiffness 26.6 – 27.8 MN.m/kg Yield strength (elastic limit) 146 – 162 MPa Tensile strength 205 – 226 MPa Specific strength 54.3 – 60.4 kN.m/kg Elongation 2.1 – 2.5 % strain Compressive strength 109 – 121 MPa … Continue reading Aluminum, 356.0, sand cast, T6 | Mechanical Properties