Composition Overview of Aluminum 356.0, sand cast, T6
| Property | Value |
|---|---|
| Compositional Summary | Al 90-93 / Si 6.5-7.5 / Mg 0.2-0.45 |
| Impurities | Fe < 0.6, Mn < 0.35, Zn < 0.35, Cu < 0.25, Ti < 0.25, Other < 0.15 |
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
| Composition Overview of Aluminum 356.0, sand cast, T6 | Composition Overview of Aluminum EN AC-Al Si7Mg sand cast T6 |
Composition detail for Aluminum 356.0, sand cast, T6
| Element | Composition Range |
|---|---|
| Al (aluminum) | 90.1% – 93.3% |
| Cu (copper) | 0% – 0.25% |
| Fe (iron) | 0% – 0.6% |
| Mg (magnesium) | 0.2% – 0.45% |
| Mn (manganese) | 0% – 0.35% |
| Si (silicon) | 6.5% – 7.5% |
| Ti (titanium) | 0% – 0.25% |
| Zn (zinc) | 0% – 0.35% |
| Other | 0% – 0.15% |
| Composition detail for Aluminum 356.0, sand cast, T6 | Composition detail for Aluminum EN AC-Al Si7Mg sand cast T6 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey