Mechanical properties of Aluminum 356.0, sand cast, T6
| Property | Value Range |
|---|---|
| Young’s modulus | 71.5 – 74.5 GPa |
| Specific stiffness | 26.6 – 27.8 MN.m/kg |
| Yield strength (elastic limit) | 146 – 162 MPa |
| Tensile strength | 205 – 226 MPa |
| Specific strength | 54.3 – 60.4 kN.m/kg |
| Elongation | 2.1 – 2.5 % strain |
| Compressive strength | 109 – 121 MPa |
| Flexural modulus | 71.5 – 74.5 GPa |
| Flexural strength (modulus of rupture) | 146 – 162 MPa |
| Shear modulus | 26.7 – 28.2 GPa |
| Bulk modulus | 66.9 – 76.6 GPa |
| Poisson’s ratio | 0.322 – 0.338 |
| Shape factor | 36 |
| Hardness – Vickers | 83 – 91 HV |
| Elastic stored energy (springs) | 146 – 180 kJ/m³ |
| Fatigue strength at 10^7 cycles | 53.1 – 64.9 MPa |
| Fatigue strength model (stress range) | 51.3 – 67.2 MPa |
| Aluminum 356.0 sand cast T6 Mechanical Properties |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey