Compositional Summary for Aluminum 354.0 T6
| Composition Summary | Details |
|---|---|
| Al87-89 / Si8.6-9.4 / Cu1.6-2 / Mg0.4-0.6 | Impurities: Fe<0.2, Ti<0.2, Mn<0.1, Zn<0.1 |
| Aluminum, 354.0, cast, T6 Composition Summary |
| Material Family | Base Material |
|---|---|
| Metal (non-ferrous) | Al (Aluminum) |
Composition Detail of Aluminum 354.0 T6
| Element | Composition Range (%) |
|---|---|
| Al (Aluminum) | 87.4 – 89.4 |
| Cu (Copper) | 1.6 – 2.0 |
| Fe (Iron) | 0.0 – 0.2 |
| Mg (Magnesium) | 0.4 – 0.6 |
| Mn (Manganese) | 0.0 – 0.1 |
| Si (Silicon) | 8.6 – 9.4 |
| Ti (Titanium) | 0.0 – 0.2 |
| Zn (Zinc) | 0.0 – 0.1 |