Mechanical Properties for Aluminum 336.0 (T65)
| Property | Value Range | Unit |
|---|---|---|
| Young’s Modulus | 72.5 – 75.5 | GPa |
| Specific Stiffness | 26.7 – 27.9 | MN·m/kg |
| Yield Strength (Elastic Limit) | 281 – 311 | MPa |
| Tensile Strength | 309 – 341 | MPa |
| Specific Strength | 103 – 115 | kN·m/kg |
| Elongation | 1 – 2 | % strain |
| Compressive Strength | 281 – 311 | MPa |
| Flexural Modulus | 73.5 – 76.5 | GPa |
| Flexural Strength (Modulus of Rupture) | 281 – 311 | MPa |
| Shear Modulus | 27.5 – 28.9 | GPa |
| Bulk Modulus | 68.8 – 78.7 | GPa |
| Poisson’s Ratio | 0.322 – 0.338 | – |
| Shape Factor | 24 | – |
| Hardness – Vickers | 135 – 150 | HV |
| Elastic Stored Energy (Springs) | 534 – 653 | kJ/m³ |
| Fatigue Strength at 10⁷ Cycles | 134 – 143 | MPa |
| Fatigue Strength Model (Stress Range) | 125 – 153 | MPa |