Aluminum, 332.0, permanent mold cast, T5 | Mechanical Properties

Mechanical Properties

PropertyMin ValueMax ValueUnit
Young’s Modulus75.578.5GPa
Specific Stiffness27.228.4MN·m/kg
Yield Strength (Elastic Limit)184204MPa
Tensile Strength237262MPa
Specific Strength66.573.7kN·m/kg
Elongation1.01.2% strain
Compressive Strength184204MPa
Flexural Modulus75.578.5GPa
Flexural Strength (Modulus of Rupture)194195MPa
Shear Modulus28.229.7GPa
Bulk Modulus70.780.8GPa
Poisson’s Ratio0.3220.338—
Shape Factor33——
Hardness (Vickers)100112HV
Elastic Stored Energy (Springs)221269kJ/m³
Fatigue Strength at 10⁷ Cycles8199MPa
Fatigue Strength Model (Stress Range)78.1103MPa
Aluminum, 332.0, permanent mold cast, T5 | Mechanical PropertiesUNS A03320 Mechanical Properties