Aluminum, 319.0, sand cast, T6 | Equivalent Grades

Standards with Similar Compositions

CountryStandardDesignation
AustraliaAS 1874AA339
IndiaIS 202 or IS 6174320
ItalyUNI7369/4SG-AlSi6Cu4
JapanJIS H5202, JIS H2211AC2B, AC2B.1
USAASTM B108, ASTM B26/B26M, ASTM B618319
ASTM B179, QQ A-371F319.1, 319.2
SAE J452A03190
—A319.0, A319.1
UNS StandardsUNS A03190, UNS A03191, UNS A13190, UNS A13191
Aluminum, 319.0, sand cast, T6 | Equivalent GradesEN AC-45200 / EN AC-Al Si6Cu4 T6 | Equivalent Grades

Tradenames
ALLCAST 51
GM-4227 M
USCO 319.1
Aluminum, 319.0, sand cast, T6 | Tradenames
EN AC-45200 / EN AC-Al Si6Cu4 T6 | Tradenames
UNS A03190 Tradenames