Aluminum, 319.0, sand cast, T6 | Mechanical Properties

Mechanical Properties

PropertyMinimumMaximumUnits
Young’s Modulus72.575.5GPa
Specific Stiffness25.927.1MN·m/kg
Yield Strength (Elastic Limit)156172MPa
Tensile Strength250275MPa
Specific Strength55.761.6kN·m/kg
Elongation22.4% strain
Compressive Strength156172MPa
Flexural Modulus72.575.5GPa
Flexural Strength (Modulus of Rupture)164180MPa
Shear Modulus27.128.6GPa
Bulk Modulus67.977.7GPa
Poisson’s Ratio0.3220.338—
Shape Factor35——
Hardness (Vickers)92102HV
Elastic Stored Energy (Springs)164200kJ/m³
Fatigue Strength at 10⁷ Cycles68.483.6MPa
Fatigue Strength Model (Stress Range)66.186.5MPa