| Country | Standard/Specification |
| Australia | AA339 to AS 1874 |
| India | 4320 to IS 202 or 617 |
| Italy | 7369/4SG-AlSi6Cu4 to UNI |
| Japan | AC2B to JIS H5202, AC2B.1 to JIS H2211 |
| USA | 319, 319 to ASTM B108, 319 to ASTM B26/B26M, 319 to ASTM B618, 319.1, 319.1 to ASTM B179, 319.1 to QQ A-371F, 319.2 to QQ A-371F, A03190 to SAE J452, A319.0, A319.1, UNS A03190, UNS A03191, UNS A13190, UNS A13191 |
| Russia | GOST 2685 AL6 |
| Aluminum, 319.0, sand cast, F | Equivalent Grades | EN AC-45200 / EN AC-Al Si6Cu4 | Equivalent Grades |
| Tradenames |
|---|
| ALLCAST 51 |
| GM-4227 M |
| USCO 319.1 |
Aluminum, 319.0, sand cast, F | General Information
Aluminum, 319.0, sand cast, F | Composition
Aluminum, 319.0, sand cast, F | Mechanical Properties
Aluminum, 319.0, sand cast, F | Equivalent Grades