Composition Overview
| Category | Details |
|---|---|
| Compositional Summary | Al 86-92 / Si 5.5-6.5 / Cu 3-4 (impurities: Fe < 1, Zn < 1, Mn < 0.5, Ni < 0.35, Ti < 0.25, Mg < 0.1, Other < 0.5) |
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
| Aluminum, 319.0, sand cast, F | Composition Overview | EN AC-45200 / EN AC-Al Si6Cu4 | Composition Overview |
Composition Details
| Element | Minimum (%) | Maximum (%) |
|---|---|---|
| Al (Aluminum) | 85.8 | 91.5 |
| Cu (Copper) | 3 | 4 |
| Fe (Iron) | 0 | 1 |
| Mg (Magnesium) | 0 | 0.1 |
| Mn (Manganese) | 0 | 0.5 |
| Ni (Nickel) | 0 | 0.35 |
| Si (Silicon) | 5.5 | 6.5 |
| Ti (Titanium) | 0 | 0.25 |
| Zn (Zinc) | 0 | 1 |
| Other | 0 | 0.5 |
| Aluminum, 319.0, sand cast, F | Composition Details | EN AC-45200 / EN AC-Al Si6Cu4 | Composition Details |
Aluminum, 319.0, sand cast, F | General Information
Aluminum, 319.0, sand cast, F | Composition
Aluminum, 319.0, sand cast, F | Mechanical Properties
Aluminum, 319.0, sand cast, F | Equivalent Grades