AISI 1117 steel (UNS G11170) is a resulfurized low carbon steel. AISI 1117 is a free-machining grade: its raised sulfur content gives short chips and fast cutting speeds. This page lists the AISI 1117 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 1117 Steel
Lightly stressed parts, e.g. camshafts, selector forks, ratchets, tappets
Compare the composition, mechanical properties and machining speed of AISI 1117 with AISI 1117, 1118, 12L14, 1137, 1141 and 1144 in our resulfurized free-machining steels comparison.
AISI 1117 Steel Parts from Turkey
Looking for AISI 1117 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1117 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.