AISI 1025 Low Carbon Steel

AISI 1025 Low Carbon Steel

AISI 1025 Steel Overview

AISI 1025 steel (UNS G10250) is a low carbon steel. This page lists the AISI 1025 material data sheets for 1 condition: normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1025 Steel

General engineering, structural and mechanical engineering.

AISI 1025 Steel Chemical Composition

C (carbon)0.22 – 0.28 %
Fe (iron)99 – 99.5 %
Mn (manganese)0.3 – 0.6 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.05 %

AISI 1025 Steel Material Data Sheets

AISI 1025 Normalized Material Data Sheet

AISI 1025 Steel Parts from Turkey

Looking for AISI 1025 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1025 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.