AISI 1117 Annealed vs As Rolled vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 1117 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength, hardness, elongation and machining speed of AISI 1117 resulfurized low carbon steel (UNS G11170) side by side for 3 conditions: annealed, as rolled, normalized. All values are taken from the individual AISI 1117 material data sheets linked below.

AISI 1117 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)Machining speed (m/min)
Annealed250–310385–475118–14026–4045.7
As Rolled275–335435–540135–16526–4042.7
Normalized270–335415–520130–16026–4045.7

AISI 1117 Differences Compared with Annealed

The table below shows how much each AISI 1117 condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength, hardness or elongation.

ConditionYield strengthTensile strengthHardnessElongation
As Rolled+9%+13%+16%+0%
Normalized+8%+9%+12%+0%

AISI 1117 Strength and Hardness Charts

AISI 1117 Yield strength by condition (MPa)Annealed250–310As Rolled275–335Normalized270–335
AISI 1117 Tensile strength by condition (MPa)Annealed385–475As Rolled435–540Normalized415–520
AISI 1117 Hardness by condition (HV)Annealed118–140As Rolled135–165Normalized130–160

AISI 1117 Heat Treatment Key Points

The highest tensile strength of AISI 1117 in these data sheets is reached in the as rolled condition (435–540 MPa). The softest condition is annealed (118–140 HV), with a machining speed of 45.7 m/min, which is usually preferred for machining and forming.

AISI 1117 is a resulfurized free-machining grade. See how it compares with the other free-machining steels in our resulfurized steels comparison.

AISI 1117 Material Data Sheets

AISI 1117 Annealed | AISI 1117 As Rolled | AISI 1117 Normalized | All AISI 1117 conditions