PARA 50% Glass Fiber Flame Retarded Material Data Sheet

PARA 50% Glass Fiber Flame Retarded (Polyarylamide) Material Data Sheet

PARA 50% Glass Fiber Flame Retarded Overview

PARA 50% glass fiber flame retarded is a grade of polyarylamide (PARA), designated Polyarylamide (50% glass fiber, flame retarded). This PARA 50% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PARA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PARA parts in-house and inspects them before shipment.

PARA 50% Glass Fiber Flame Retarded Designation

Polyarylamide (50% glass fiber, flame retarded)
TradenamesIxef, Reny

PARA 50% Glass Fiber Flame Retarded Typical uses

Automotive, furniture, small appliances, lawn mowers, power tools, electrical contactors and switches, electrical motor components, cell phones, faucet components.

PARA 50% Glass Fiber Flame Retarded Composition detail

Polymer35–45%
Flame retardant5–15%
Glass (fiber)50  %

PARA 50% Glass Fiber Flame Retarded Physical properties

Density1.75–1.79g/cm3

PARA 50% Glass Fiber Flame Retarded Mechanical properties

Young’s modulus17–21.2GPa
Specific stiffness9.6–12MN.m/kg
Yield strength (elastic limit)172–215MPa
Tensile strength182–222MPa
Specific strength97.1–122kN.m/kg
Elongation1.8–2.59% strain
Elongation at yield1.52–2.88% strain
Compressive modulus18.1–20GPa
Compressive strength230–254MPa
Flexural modulus16.6–19.9GPa
Flexural strength (modulus of rupture)272–333MPa
Shear modulus6.97–7.33GPa
Shear strength109–133MPa
Bulk modulus18–19.9GPa
Poisson’s ratio0.327–0.332 
Shape factor8.11
Hardness – Vickers55–61HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Shore D98–102 
Elastic stored energy (springs)771–1230kJ/m3
Fatigue strength at 10^7 cycles76.7–84.7MPa

PARA 50% Glass Fiber Flame Retarded Impact & fracture properties

Fracture toughness5.55–6.13MPa.m0.5
Toughness (G)1.55–2.07kJ/m2
Impact strength, notched 23 °C6.66–12.9kJ/m2
Impact strength, unnotched 23 °C28–41.2kJ/m2

PARA 50% Glass Fiber Flame Retarded Thermal properties

Melting point268–282°C
Glass temperature78–92.2°C
Heat deflection temperature 0.45MPa254–258°C
Heat deflection temperature 1.8MPa226–230°C
Vicat softening point77–90°C
Maximum service temperature187–199°C
Thermal conductivity0.629–0.644W/m.°C
Specific heat capacity1160–1180J/kg.°C
Thermal expansion coefficient16.6–17.4µstrain/°C
Thermal shock resistance510–696°C
Thermal distortion resistance0.0364–0.0385MW/m

PARA 50% Glass Fiber Flame Retarded Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)3.62–5.1 
Dissipation factor (dielectric loss tangent)0.0145–0.0381 
Dielectric strength (dielectric breakdown)21.3–36.2MV/m
Comparative tracking index400–450V

PARA 50% Glass Fiber Flame Retarded Magnetic properties

Magnetic typeNon-magnetic

PARA 50% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3090–3470m/s
Mechanical loss coefficient (tan delta)0.00588–0.0065 

PARA 50% Glass Fiber Flame Retarded Absorption & permeability

Water absorption @ 24 hrs0.17–0.28%
Water absorption @ sat1.4–1.9%
Humidity absorption @ sat1–1.4%

PARA 50% Glass Fiber Flame Retarded Processing properties

Polymer injection moldingLimited use
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.1 – 0.3 %
Melt temperature268 – 282 °C
Mold temperature118 – 141 °C
Molding pressure range30 – 150 MPa

PARA 50% Glass Fiber Flame Retarded Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsLimited use
Oils and fuelsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Good
FlammabilitySelf-extinguishing