PA12 (nylon 12) has the lowest water absorption of the polyamides, with good dimensional stability and electrical properties. It is tougher than PA11, is available in very flexible grades, and melts and processes at lower temperatures than most other grades.
PA12 Limitations
It is relatively expensive and has the lowest strength and heat resistance of the polyamides.
Typical Uses of PA12
Hydraulic and pneumatic hoses, tubing for oil, fuel and air brakes, termite-resistant cable sheathing, pipe liners and pipe rehabilitation, shoe soles and, as a fine spherical powder, cosmetics.
PA12 Compositional Summary
(NH(CH2)11-CO)n
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PA12 (Polyamide / nylon 12)
CAS number
24937-16-4
PA12 Processing Properties
Forming
Molding temperatures are low for a polyamide.
Machining
It usually machines easily, although flexible grades are harder to machine.
Joining
Flexible grades are very difficult or impossible to weld ultrasonically.
Surface Treatment
It is harder to paint than other polyamides.