PA12 Semi-Flexible Grade Material Data Sheet

PA12 Semi-Flexible Grade (Polyamide 12) Material Data Sheet

PA12 Semi-Flexible Grade Overview

PA12 semi-flexible grade is a grade of polyamide 12 (PA12, nylon 12), designated Polyamide (Nylon) (Type 12, semi-flexible, molding and extrusion). This PA12 semi-flexible grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA12 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA12 parts in-house and inspects them before shipment.

PA12 Semi-Flexible Grade Designation

Polyamide (Nylon) (Type 12, semi-flexible, molding and extrusion)
TradenamesAshlene, Grilamid, Rilsan, Ubesta, Vestamid

PA12 Semi-Flexible Grade Typical uses

Precision engineering components, components requiring low temperature toughness, sports shoe soles, pipes and tubes for automotive fuel and brake lines.

PA12 Semi-Flexible Grade Composition detail

Polymer90–95%
Plasticizer/oil5–10%

PA12 Semi-Flexible Grade Physical properties

Density1.02–1.03g/cm3

PA12 Semi-Flexible Grade Mechanical properties

Young’s modulus0.44–0.55GPa
Specific stiffness0.429–0.537MN.m/kg
Yield strength (elastic limit)28–30MPa
Tensile strength35–40MPa
Specific strength27.3–29.3kN.m/kg
Elongation340–350% strain
Elongation at yield20–25% strain
Compressive modulus0.44–0.55GPa
Compressive strength42–48MPa
Flexural modulus0.44–0.55GPa
Flexural strength (modulus of rupture)40.6–43.5MPa
Shear modulus0.16–0.19GPa
Shear strength21–24MPa
Bulk modulus0.78–1.18GPa
Poisson’s ratio0.406–0.422 
Shape factor3.3
Hardness – Vickers9–10HV
Hardness – Rockwell M57
Hardness – Rockwell R87
Hardness – Shore D64–65 
Elastic stored energy (springs)751–971kJ/m3
Fatigue strength at 10^7 cycles14–16MPa

PA12 Semi-Flexible Grade Impact & fracture properties

Fracture toughness2.73–2.85MPa.m0.5
Toughness (G)14–17.8kJ/m2
Impact strength, notched 23 °C14–18kJ/m2
Impact strength, notched -30 °C3–8kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA12 Semi-Flexible Grade Thermal properties

Melting point173–174°C
Glass temperature40–43°C
Heat deflection temperature 0.45MPa93–100°C
Heat deflection temperature 1.8MPa45–48°C
Maximum service temperature80–110°C
Minimum service temperature-67–-47°C
Thermal conductivity0.218–0.306W/m.°C
Specific heat capacity1680–1720J/kg.°C
Thermal expansion coefficient140–180µstrain/°C
Thermal shock resistance314–439°C
Thermal distortion resistance0.00132–0.002MW/m

PA12 Semi-Flexible Grade Electrical properties

Electrical resistivity7e17–1e19µohm.cm
Electrical conductivity1.72e-17–2.46e-16%IACS
Dielectric constant (relative permittivity)3.3–10 
Dissipation factor (dielectric loss tangent)0.14–0.19 
Dielectric strength (dielectric breakdown)26–32MV/m
Comparative tracking index600  V

PA12 Semi-Flexible Grade Magnetic properties

Magnetic typeNon-magnetic

PA12 Semi-Flexible Grade Optical, aesthetic and acoustic properties

Refractive index1.52–1.54 
TransparencyTranslucent
Acoustic velocity654–734m/s
Mechanical loss coefficient (tan delta)0.1–0.125 

PA12 Semi-Flexible Grade Absorption & permeability

Water absorption @ 24 hrs0.2  %
Water absorption @ sat1.2–1.5%
Humidity absorption @ sat0.65–0.7%
Water vapor transmission0.29  g.mm/m².day
Permeability (O2)32  cm³.mm/m².day.atm

PA12 Semi-Flexible Grade Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.8 – 1.25 %
Melt temperature230 – 260 °C
Mold temperature40 – 80 °C
Molding pressure range16 – 75 MPa

PA12 Semi-Flexible Grade Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsAcceptable
Oils and fuelsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilityHighly flammable