Home » PA (Polyamide / Nylon) » PA612 (Polyamide 612 / Nylon 612) » PA612 Glass Filled Grades » PA612 33% Glass Fiber Toughened Material Data Sheet
PA612 33% Glass Fiber Toughened (Polyamide 612) Material Data Sheet
PA612 33% Glass Fiber Toughened Overview
PA612 33% glass fiber toughened is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 33% Glass Fiber, Toughened). This PA612 33% glass fiber toughened material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 33% Glass Fiber Toughened Designation
Polyamide (Nylon) (Type 612, 33% Glass Fiber, Toughened) Tradenames Akromid, Edgetek, Grilamid, Technyl, Ultramid, Zytel
PA612 33% Glass Fiber Toughened Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 33% Glass Fiber Toughened Composition detail
Polymer 52 – 64 % Impact modifier 3 – 15 % Glass (fiber) 33 %
PA612 33% Glass Fiber Toughened Physical properties
PA612 33% Glass Fiber Toughened Mechanical properties
Young’s modulus 5.86 – 7.31 GPa Specific stiffness 4.65 – 5.8 MN.m/kg Yield strength (elastic limit) 114 – 142 MPa Tensile strength 115 – 141 MPa Specific strength 90.5 – 113 kN.m/kg Elongation 2.64 – 3.8 % strain Elongation at yield 2.22 – 4.22 % strain Compressive modulus 6.26 – 6.92 GPa Compressive strength 146 – 162 MPa Flexural modulus 5.27 – 6.31 GPa Flexural strength (modulus of rupture) 171 – 209 MPa Shear modulus 2.34 – 2.46 GPa Shear strength 69.3 – 84.6 MPa Bulk modulus 8.22 – 9.08 GPa Poisson’s ratio 0.358 – 0.373 Shape factor 5.39 Hardness – Vickers 37 – 40 HV Hardness – Rockwell M 163 – 181 Hardness – Rockwell R 163 – 181 Hardness – Shore D 93 – 97 Elastic stored energy (springs) 982 – 1560 kJ/m3 Fatigue strength at 10^7 cycles 48.7 – 53.9 MPa
PA612 33% Glass Fiber Toughened Impact & fracture properties
Fracture toughness 4.48 – 4.95 MPa.m0.5 Toughness (G) 2.93 – 3.91 kJ/m2 Impact strength, notched 23 °C 10.2 – 19.8 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 64.8 – 95.2 kJ/m2 Impact strength, unnotched -30 °C 42 – 63 kJ/m2
PA612 33% Glass Fiber Toughened Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 199 – 247 °C Heat deflection temperature 1.8MPa 174 – 220 °C Maximum service temperature 47 – 67 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.396 – 0.412 W/m.°C Specific heat capacity 1470 – 1530 J/kg.°C Thermal expansion coefficient 57.6 – 58.7 µstrain/°C Thermal shock resistance 287 – 389 °C Thermal distortion resistance 0.00679 – 0.0071 MW/m
PA612 33% Glass Fiber Toughened Electrical properties
Electrical resistivity 2.73e21 – 6.83e22 µohm.cm Electrical conductivity 2.52e-21 – 6.32e-20 %IACS Dielectric constant (relative permittivity) 4.57 – 6.44 Dissipation factor (dielectric loss tangent) 0.0223 – 0.0587 Dielectric strength (dielectric breakdown) 20.4 – 34.7 MV/m Comparative tracking index 600 V
PA612 33% Glass Fiber Toughened Magnetic properties
Magnetic type Non-magnetic
PA612 33% Glass Fiber Toughened Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2150 – 2410 m/s Mechanical loss coefficient (tan delta) 0.0104 – 0.0115
PA612 33% Glass Fiber Toughened Absorption & permeability
Water absorption @ 24 hrs 0.38 – 0.61 % Water absorption @ sat 1.7 – 2.2 % Humidity absorption @ sat 0.7 – 0.95 %
PA612 33% Glass Fiber Toughened Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.5 % Melt temperature 212 – 293 °C Mold temperature 30 – 60 °C Molding pressure range 27.5 – 138 MPa
PA612 33% Glass Fiber Toughened Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning