Home » PA (Polyamide / Nylon) » PA612 (Polyamide 612 / Nylon 612) » PA612 Unfilled Grades » PA612 Molding Grade Material Data Sheet
PA612 Molding Grade (Polyamide 612) Material Data Sheet
PA612 Molding Grade Overview
PA612 molding grade is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, Molding). This PA612 molding grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 Molding Grade Designation
Polyamide (Nylon) (Type 612, Molding) Tradenames Ashlene, Badamid, Comco, Electrafil, Grilamid, Grilon, Hiprolon, Isocor, Lubriblend, Nycal, Nycast, Plaslube, Schulamid, Shandong, Vestamid, Zytel
PA612 Molding Grade Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 Molding Grade Composition detail
PA612 Molding Grade Physical properties
PA612 Molding Grade Mechanical properties
Young’s modulus 1.43 – 1.79 GPa Specific stiffness 1.35 – 1.69 MN.m/kg Yield strength (elastic limit) 47.1 – 58.7 MPa Tensile strength 59.5 – 72.7 MPa Specific strength 44.4 – 55.4 kN.m/kg Elongation 34.9 – 50.3 % strain Elongation at yield 13.3 – 25.2 % strain Compressive modulus 1.53 – 1.69 GPa Compressive strength 75.4 – 83.3 MPa Flexural modulus 1.53 – 1.83 GPa Flexural strength (modulus of rupture) 80.7 – 98.6 MPa Shear modulus 0.555 – 0.584 GPa Shear strength 35.7 – 43.6 MPa Bulk modulus 3 – 3.32 GPa Poisson’s ratio 0.399 – 0.415 Shape factor 4.1 Hardness – Vickers 15 – 17 HV Hardness – Rockwell M 117 – 129 Hardness – Rockwell R 117 – 129 Hardness – Shore D 92 – 95 Elastic stored energy (springs) 685 – 1090 kJ/m3 Fatigue strength at 10^7 cycles 25.1 – 27.8 MPa
PA612 Molding Grade Impact & fracture properties
Fracture toughness 3.37 – 3.72 MPa.m0.5 Toughness (G) 6.78 – 9.06 kJ/m2 Impact strength, notched 23 °C 5.01 – 9.72 kJ/m2 Impact strength, notched -30 °C 3.33 – 7.24 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA612 Molding Grade Thermal properties
Melting point 195 – 219 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 155 – 166 °C Heat deflection temperature 1.8MPa 58 – 82 °C Maximum service temperature 90 – 120 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.209 – 0.226 W/m.°C Specific heat capacity 1580 – 1600 J/kg.°C Thermal expansion coefficient 89.1 – 90.9 µstrain/°C Thermal shock resistance 313 – 426 °C Thermal distortion resistance 0.00232 – 0.00251 MW/m
PA612 Molding Grade Electrical properties
Electrical resistivity 1.32e19 – 3.3e20 µohm.cm Electrical conductivity 5.22e-19 – 1.31e-17 %IACS Dielectric constant (relative permittivity) 4.26 – 6.01 Dissipation factor (dielectric loss tangent) 0.0431 – 0.114 Dielectric strength (dielectric breakdown) 23.5 – 40.1 MV/m Comparative tracking index 600 V
PA612 Molding Grade Magnetic properties
Magnetic type Non-magnetic
PA612 Molding Grade Optical, aesthetic and acoustic properties
Transparency Translucent Acoustic velocity 1160 – 1300 m/s Mechanical loss coefficient (tan delta) 0.0194 – 0.0214
PA612 Molding Grade Absorption & permeability
Water absorption @ 24 hrs 0.54 – 0.88 % Water absorption @ sat 2.4 – 3.1 % Humidity absorption @ sat 1 – 1.4 % Permeability (O2) 36.5 – 86 cm³.mm/m².day.atm
PA612 Molding Grade Processing properties
Polymer injection molding Excellent Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.21 % Melt temperature 232 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 6.88 – 103 MPa
PA612 Molding Grade Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning