PA46 30% Glass Fiber Flame Retarded Material Data Sheet

PA46 30% Glass Fiber Flame Retarded (Polyamide 46) Material Data Sheet

PA46 30% Glass Fiber Flame Retarded Overview

PA46 30% glass fiber flame retarded is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, 30% Glass Fiber, V-0). This PA46 30% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.

PA46 30% Glass Fiber Flame Retarded Designation

Polyamide (Nylon) (Type 46, 30% Glass Fiber, V-0)
TradenamesHifill, Stanyl

PA46 30% Glass Fiber Flame Retarded Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA46 30% Glass Fiber Flame Retarded Composition detail

Polymer55–65%
Flame retardant5–15%
Glass (fiber)30  %

PA46 30% Glass Fiber Flame Retarded Physical properties

Density1.62–1.65g/cm3

PA46 30% Glass Fiber Flame Retarded Mechanical properties

Young’s modulus7.12–8.88GPa
Specific stiffness4.35–5.43MN.m/kg
Yield strength (elastic limit)111–139MPa
Tensile strength113–138MPa
Specific strength67.9–85kN.m/kg
Elongation2.87–4.13% strain
Elongation at yield2.42–4.59% strain
Compressive modulus7.6–8.4GPa
Compressive strength143–158MPa
Flexural modulus6.53–7.82GPa
Flexural strength (modulus of rupture)165–202MPa
Shear modulus2.87–3.01GPa
Shear strength67.5–82.5MPa
Bulk modulus9.05–10GPa
Poisson’s ratio0.346–0.36 
Shape factor6.13
Hardness – Vickers36–39HV
Hardness – Rockwell M161–178 
Hardness – Rockwell R161–178 
Hardness – Shore D93–97 
Elastic stored energy (springs)767–1230kJ/m3
Fatigue strength at 10^7 cycles47.5–52.5MPa

PA46 30% Glass Fiber Flame Retarded Impact & fracture properties

Fracture toughness4.66–5.15MPa.m0.5
Toughness (G)2.61–3.49kJ/m2
Impact strength, notched 23 °C7.48–14.5kJ/m2
Impact strength, notched -30 °C6.3–13.7kJ/m2
Impact strength, unnotched 23 °C48.6–71.4kJ/m2
Impact strength, unnotched -30 °C40–60kJ/m2

PA46 30% Glass Fiber Flame Retarded Thermal properties

Melting point284–306°C
Glass temperature71–79°C
Heat deflection temperature 0.45MPa284–340°C
Heat deflection temperature 1.8MPa258–313°C
Maximum service temperature73–87°C
Minimum service temperature-58–-38°C
Thermal conductivity0.507–0.527W/m.°C
Specific heat capacity1210–1260J/kg.°C
Thermal expansion coefficient37.4–38.2µstrain/°C
Thermal shock resistance354–482°C
Thermal distortion resistance0.0134–0.014MW/m

PA46 30% Glass Fiber Flame Retarded Electrical properties

Electrical resistivity1.51e15–3.76e16µohm.cm
Electrical conductivity4.59e-15–1.14e-13%IACS
Dielectric constant (relative permittivity)8.3–11.7 
Dissipation factor (dielectric loss tangent)0.182–0.479 
Dielectric strength (dielectric breakdown)14.8–25.2MV/m
Comparative tracking index300–350V

PA46 30% Glass Fiber Flame Retarded Magnetic properties

Magnetic typeNon-magnetic

PA46 30% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2080–2330m/s
Mechanical loss coefficient (tan delta)0.00938–0.0104 

PA46 30% Glass Fiber Flame Retarded Absorption & permeability

Water absorption @ 24 hrs1.2–2%
Water absorption @ sat4.9–6.5%
Humidity absorption @ sat1.4–1.9%

PA46 30% Glass Fiber Flame Retarded Processing properties

Polymer injection moldingAcceptable
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.4 – 0.6 %
Melt temperature242 – 316 °C
Mold temperature40 – 80 °C
Molding pressure range34.4 – 103 MPa

PA46 30% Glass Fiber Flame Retarded Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySelf-extinguishing