Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Carbon Filled Grades » PA66 15% Nickel-Coated Carbon Fiber Material Data Sheet
PA66 15% Nickel-Coated Carbon Fiber (Polyamide 66) Material Data Sheet
PA66 15% Nickel-Coated Carbon Fiber Overview
PA66 15% nickel-coated carbon fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 15% Nickel-coated Carbon Fiber, Conductive – EMI Shielding). This PA66 15% nickel-coated carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 15% Nickel-Coated Carbon Fiber Designation
Polyamide (Nylon) (Type 66, 15% Nickel-coated Carbon Fiber, Conductive – EMI Shielding) Tradenames Alamid, Electrablend, LNP Thermocomp, Staramide
PA66 15% Nickel-Coated Carbon Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 15% Nickel-Coated Carbon Fiber Composition detail
Polymer 85 % Carbon (fiber) 15 %
PA66 15% Nickel-Coated Carbon Fiber Physical properties
PA66 15% Nickel-Coated Carbon Fiber Mechanical properties
Young’s modulus 6.36 – 7.94 GPa Specific stiffness 5.01 – 6.25 MN.m/kg Yield strength (elastic limit) 62.9 – 78.5 MPa Tensile strength 76.3 – 93.3 MPa Specific strength 49.5 – 61.8 kN.m/kg Elongation 2.06 – 2.97 % strain Elongation at yield 1.65 – 3.13 % strain Compressive modulus 6.79 – 7.51 GPa Compressive strength 96.7 – 107 MPa Flexural modulus 5.38 – 6.44 GPa Flexural strength (modulus of rupture) 108 – 132 MPa Shear modulus 2.54 – 2.67 GPa Shear strength 45.8 – 56 MPa Bulk modulus 8.77 – 9.7 GPa Poisson’s ratio 0.357 – 0.371 Shape factor 8.3 Hardness – Vickers 20 – 22 HV Hardness – Rockwell M 133 – 147 Hardness – Rockwell R 133 – 147 Hardness – Shore D 86 – 90 Elastic stored energy (springs) 275 – 438 kJ/m3 Fatigue strength at 10^7 cycles 32.2 – 35.6 MPa
PA66 15% Nickel-Coated Carbon Fiber Impact & fracture properties
Fracture toughness 4.55 – 5.03 MPa.m0.5 Toughness (G) 2.79 – 3.72 kJ/m2 Impact strength, notched 23 °C 12.5 – 24.2 kJ/m2 Impact strength, notched -30 °C 8.85 – 19.2 kJ/m2
PA66 15% Nickel-Coated Carbon Fiber Thermal properties
Melting point 260 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 238 – 290 °C Heat deflection temperature 1.8MPa 213 – 263 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.394 – 0.41 W/m.°C Specific heat capacity 1530 – 1600 J/kg.°C Thermal expansion coefficient 58.2 – 59.3 µstrain/°C Thermal shock resistance 144 – 196 °C Thermal distortion resistance 0.00669 – 0.00699 MW/m
PA66 15% Nickel-Coated Carbon Fiber Electrical properties
Electrical resistivity 2e6 – 5e7 µohm.cm Electrical conductivity 3.45e-6 – 8.62e-5 %IACS Galvanic potential 0.14 – 0.22 V
PA66 15% Nickel-Coated Carbon Fiber Magnetic properties
Magnetic type Non-magnetic
PA66 15% Nickel-Coated Carbon Fiber Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2230 – 2500 m/s Mechanical loss coefficient (tan delta) 0.0103 – 0.0114
PA66 15% Nickel-Coated Carbon Fiber Absorption & permeability
Water absorption @ 24 hrs 0.49 – 0.8 % Water absorption @ sat 5.6 – 7.5 % Humidity absorption @ sat 1.6 – 2.2 %
PA66 15% Nickel-Coated Carbon Fiber Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.455 – 0.55 % Melt temperature 223 – 299 °C Mold temperature 40 – 60 °C Molding pressure range 68.8 – 138 MPa
PA66 15% Nickel-Coated Carbon Fiber Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning