Modified PEEK Unfilled Grade Material Data Sheet

Modified PEEK Unfilled Grade (Polyetheretherketone) Material Data Sheet

Modified PEEK Unfilled Grade Overview

Modified PEEK unfilled grade is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (unfilled). This modified PEEK unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

Modified PEEK Designation

Modified poly(etheretherketone) (unfilled)
TradenamesLatigray, Latiohm, LNP Lubricomp, LNP Stat-Kon, LNP Thermocomp, Lubricomp, Optestat, Thermocomp

Modified PEEK Unfilled Grade Composition detail

Polymer100  %

Modified PEEK Physical properties

Density1.29–1.31g/cm3

Modified PEEK Unfilled Grade Mechanical properties

Young’s modulus2.69–3.51GPa
Specific stiffness2.07–2.7MN.m/kg
Yield strength (elastic limit)70–75MPa
Tensile strength81.8–88.8MPa
Specific strength53.8–57.8kN.m/kg
Elongation28.8–43.8% strain
Elongation at yield5.28–6.52% strain
Compressive modulus2.69–3.51GPa
Flexural modulus2.8–3.55GPa
Flexural strength (modulus of rupture)117–136MPa
Shear modulus1–1.3GPa
Shear strength75.5–83.5MPa
Poisson’s ratio0.39–0.43 
Shape factor4.9
Hardness – Vickers21–22HV
Elastic stored energy (springs)738–989kJ/m3
Fatigue strength at 10^7 cycles32.4–35.8MPa

Modified PEEK Impact & fracture properties

Impact strength, notched 23 °C7.16–9.84kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2

Modified PEEK Unfilled Grade Thermal properties

Melting point613–618°C
Glass temperature149–167°C
Heat deflection temperature 0.45MPa445–538°C
Heat deflection temperature 1.8MPa434–525°C
Vicat softening point445–538°C
Thermal conductivity0.2–0.24W/m.°C
Specific heat capacity1520–1560J/kg.°C
Thermal expansion coefficient45–47µstrain/°C
Thermal shock resistance447–588°C
Thermal distortion resistance0.00434–0.00523MW/m

Modified PEEK Electrical properties

Electrical resistivity25000000000000000–100000000000000000µohm.cm
Electrical conductivity1.72e-15–6.9e-15%IACS
Dielectric constant (relative permittivity)3.3–4 
Dissipation factor (dielectric loss tangent)0.001–0.006 
Dielectric strength (dielectric breakdown)30–70MV/m

Modified PEEK Magnetic properties

Magnetic typeNon-magnetic

Modified PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1440–1650m/s

Modified PEEK Absorption & permeability

Water absorption @ 24 hrs0.1–0.2%
Water absorption @ sat0.45–0.55%

Modified PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionAcceptable
Polymer thermoformingUnsuitable
Linear mold shrinkage1.1 – 1.5 %
Melt temperature366 – 388 °C
Mold temperature149 – 204 °C

Modified PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing