General purpose copper covers the deoxidized and tough-pitch copper grades such as C12200, C12500 and C14200, used where very high conductivity is not the only requirement.
GP Copper Strengths
It combines high ductility with high thermal and electrical conductivity, reasonable strength, good corrosion resistance, excellent durability and an attractive appearance.
GP Copper Limitations
The material is very soft and has a high density.
GP Copper Designation
Typical grades are C12200, C12500 and C14200, which are deoxidized coppers.
Typical Uses of GP Copper
Electrical wiring, conductors, cables, overhead and contact wires, heat exchangers, boilers and pressure vessels, roofing and architectural work, cookware and coins.
GP Copper Compositional Summary
Copper with varying additions of phosphorus and arsenic; residual oxygen levels vary
Material family
Metal (non-ferrous)
Base material
Cu (Copper)
GP Copper Microstructure
Single-phase alpha structure with a face-centred cubic lattice.
Effect of Composition on GP Copper
Removing impurities generally raises electrical and thermal conductivity. Silver is the only addition that increases conductivity.
GP Copper Processing Properties
Forming
Formability is good.
Machining
Machinability is good.
Joining
It is easy to join, but its high ductility normally prevents spot welding.