AISI 405 Stainless Steel Similar Compositions

AISI 405 Stainless Steel Similar Compositions

Australia: 405 to AS 1449
Bulgaria: 0Ch13Ju to BDS 6738
Canada: 405 to CSA G110.3, 405 to CSA G110.5, 405 to CSA G110.9
China: 0Cr13Al to GB 1220, 0Cr13Al to GB 1221, 0Cr13Al to GB 4237, 0Cr13Al to GB 4238, 0Cr13Al to GB/T 12771, 0Cr13Al to GB/T 17102, 0Cr13Al to GB/T 3280, 0Cr13Al to GB/T 4239, 0Cr13Al to GB/T 6725
Germany: 1.4002 to DIN 17440, 1.4002 to DIN 17441, 1.4002 to DIN EN 10088, X6CrAl13 to DIN EN 10088
India: X04Cr13 to IS 6527, X04Cr13A to IS 6528
International: 2 to ISO 683-13
Italy: X6CrAl13 to UNI 6901, X6CrAl13 to UNI 6904
Japan: SUS405 to JIS G4303, SUS405 to JIS G4304, SUS405 to JIS G4305, SUS405 to JIS G4306, SUS405 to JIS G4307, SUS405 to JIS G4309, SUS405TB to JIS G3463, SUS405TP to JIS G3459
Mexico: 405 to NMX-B-83, MT405 to NMX-B-171
Poland: 0H13J to PN-H-86020
Romania: 7AlCr130 to STAS 3583
South Korea: STS 405 to KS D 3706, STS 405-W2 to KS D 3703, STS405 to KS D 3698, STS405 to KS D 3705
Spain: E-405 to UNE 36016/1, F.3111 to UNE 36016, F.3111 to UNE 36016/1, X6CrAl13 to UNE 36016
UK: 405S17 to BS 1449/2, 405S17 to BS 1503, X6CrAl13 to BS EN 10250-4
USA: 405 to ASTM A176-99, 405 to ASTM A314-97, 405 to ASTM A473, 405 to DoD-F-24669/7, 405 to FED QQ-S-763F, 405 to MIL-S-861, 405 to MIL-S-862B, MT405 to ASTM A511, S40500 to ASTM A240/A240M, S40500 to ASTM A276, S40500 to ASTM A479/A479M, S40500 to ASTM A580/A580M-98, S40500 to ASTM A959, S40500 to SAE J405, TP405 to ASTM A268/A268M, UNS S40500
Tradenames:
ALLEGHENY ATAINLESS TYPE 405, ALLEGHENY LUDLUM TYPE 405, ARMCO 400, SPARTAN REDHEUGH 405S17

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey