AISI 405 Stainless Steel Mechanical Properties (Ferritic, Annealed, Low Nickel)

Young’s modulus195–205GPa
Specific stiffness25.2–26.7MN.m/kg
Yield strength (elastic limit)170–275MPa
Tensile strength415–480MPa
Specific strength22–35.7kN.m/kg
Elongation17–25% strain
Compressive strength170–275MPa
Flexural modulus195–205GPa
Flexural strength (modulus of rupture)170–275MPa
Shear modulus75–81GPa
Bulk modulus144–159GPa
Poisson’s ratio0.275–0.285 
Shape factor64   
Hardness – Vickers150–200HV
Hardness – Rockwell B71–79HRB
Hardness – Rockwell C0–11HRC
Hardness – Brinell150–192HB
Elastic stored energy (springs)75.7–181kJ/m^3
Fatigue strength at 10^7 cycles231–257MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles209–284MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey