AISI 405 Stainless Steel Designation
AISI 405 Stainless Steel , Ferritic, Annealed, Low Nickel AISI 405, wrought Condition Annealed or annealed and cold finished UNS number S40500 US name ASTM S40500, ASTM MT405 EN name X6CrAl13 EN number 1.4002 GB (Chinese) name 0Cr13Al JIS (Japanese) name Symbol SUS405, SUS405 MODULUS METALSand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting … Continue reading AISI 405 Stainless Steel Designation