AISI 405 Stainless Steel Mechanical Properties
AISI 405 Stainless Steel Mechanical Properties (Ferritic, Annealed, Low Nickel) Young’s modulus 195 – 205 GPa Specific stiffness 25.2 – 26.7 MN.m/kg Yield strength (elastic limit) 170 – 275 MPa Tensile strength 415 – 480 MPa Specific strength 22 – 35.7 kN.m/kg Elongation 17 – 25 % strain Compressive strength 170 – 275 MPa Flexural … Continue reading AISI 405 Stainless Steel Mechanical Properties