EN GJL 200 Cast Iron Thermal Properties (Gray, flake graphite)
| Melting point | 1130 | – | 1240 | °C |
| Maximum service temperature | 350 | – | 450 | °C |
| Minimum service temperature | -150 | – | -50 | °C |
| Thermal conductivity | 46 | – | 56 | W/m.°C |
| Specific heat capacity | 460 | – | 500 | J/kg.°C |
| Thermal expansion coefficient | 11 | – | 13 | µstrain/°C |
| Thermal shock resistance | 91 | – | 116 | °C |
| Thermal distortion resistance | 3.74 | – | 4.82 | MW/m |
| Latent heat of fusion | 270 | – | 275 | kJ/kg |
EN GJL 200 Similar Compositions
| India: |
| FG 200 to IS 6331, FG 260 to IS 6331 |
| Russia: |
| VSH 500-2 to GOST 3925, VSH 600-3 to GOST 3925, VSH 700-2 to GOST 3925, VSH 800-2 to GOST 3925, VSH 900-2 to GOST 3925 |
| USA: |
| A-CA to ASTM A823-99, A-CB to ASTM A823-99, A-CC to ASTM A823-99, A-SA to ASTM A823-99, A-SB to ASTM A823-99, A-SC to ASTM A823-99, A-SS to ASTM A823-99, G10H18 to SAE J431, G10H21 c to SAE J431, G11H18 to SAE J431, G11H20 b to SAE J431, G11H20 to SAE J431, G12H21 to SAE J431, G13H19 to SAE J431, G1800 to SAE J431, G2500 to ASTM A159-83, G2500 to SAE J431, G3000 to ASTM A159-83, G3000 to SAE J431, G3500 to SAE J431, G4000 to SAE J431, G9H12 to SAE J431, G9H17 a to SAE J431, G9H17 to SAE J431, N-CA to ASTM A823-99, N-CB to ASTM A823-99, N-CC to ASTM A823-99, N-SA to ASTM A823-99, N-SB to ASTM A823-99, N-SC to ASTM A823-99, N-SS to ASTM A823-99, SPVG10 to SAE J1682, SPVG12 to SAE J1682, UNS F10005, UNS F10006 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey